Desulfurization and demineralization of asphaltite by aqueous caustic leaching
[ X ]
Tarih
2007
Yazarlar
Dergi Başlığı
Dergi ISSN
Cilt Başlığı
Yayıncı
Estonian Acad Publishers
Erişim Hakkı
info:eu-repo/semantics/closedAccess
Özet
The method of desulfurization and demineralization by aqueous caustic leaching (ACL) was used for treatment of asphaltite samples front Seguruk collieries of Sirnak asphaltite fields, situated in Southeast Anatolia region of Turkey. The effect of different parameters such as alkali concentration, time and temperature on leaching efficiency was studied, and the experimental results are presented here. The concentration of caustic was varied from 0.1 to 1.0 M, temperature from 100 to 180 degrees C, and leaching time from 4 to 16 h. Elevation of alkali concentration, leaching temperature and prolongation of time increase the removal of total sulfur and ash. As a result of ACL, ash content of asphaltite was reduced from 40.08 to 22.14%, and 75% of combustible was recovered. Total sulfur and volatile matter content was reduced from 6.74 to 2.49% and from 33.72 to 19.10%, respectively.
Açıklama
Anahtar Kelimeler
[No Keyword]
Kaynak
Oil Shale
WoS Q Değeri
Q2
Scopus Q Değeri
Q2
Cilt
24
Sayı
3