The contribution of ceramic thickness and adhesive type on the de-bonding strength of dental ceramic veneers using er,cr:Ysgg laser

dc.authorid0000-0001-5466-7247en_US
dc.authorid0000-0003-2975-4511en_US
dc.contributor.authorYılmaz, Berivan Dündar
dc.contributor.authorPolat, Zelal Seyfioǧlu
dc.contributor.authorİzgi, Ayça Deniz
dc.contributor.authorGündüz, Derya Toprak
dc.contributor.authorDirihan, Roda Seseogullari
dc.date.accessioned2022-04-29T06:52:32Z
dc.date.available2022-04-29T06:52:32Z
dc.date.issued2019en_US
dc.departmentDicle Üniversitesi, Diş Hekimliği Fakültesi, Protetik Diş Tedavisi Bölümüen_US
dc.description.abstractPurpose: De-bonding strength of ceramic veneers by laser use needs to be evaluated in detail. The aim of this study, is to determine the contribution of ceramic thickness and cementing agents to the de-bonding strength of ceramic veneers using Er,Cr:YSGG laser. Methods: A total of 120 maxillary central incisors specimens were randomly divided into twelve groups on the basis of disc thickness, cementing agent, and Er,Cr:YSGG laser use. Under laboratory conditions, 120 IPS Empress II system discs 0.5mm, 1mm, and 2mm in thickness were applied to the tooth surfaces, for laser use. An Er,Cr:YSGG laser system was applied to the central surface of the IPS Empress II discs on specimens in all laser groups (Groups 1,3,5,7,9,11). Then the shear bond strength (SBS) for all specimens were tested with a testing machine at a speed of 0.5mm/min. The SBS values were considered as the de-bonding strength. Results: The mean de-bonding strength values for Groups 9 and 11 (0,5 mm disc thickness + laser application) have the lowest median load (0.000 N), while Group 4 (2mm disc thickness + no laser) has the highest median load (573.885 N). The de-bonding strengths of all the groups without laser application were higher than those of all groups with laser use. When laser is applied, the mean de-bonding strength decreases with decreasing disc thickness, and it reaches zero at 0.5mm thickness of discs cemented by self- or total-etch adhesives. Conclusions: The de-bonding strength decreases with laser use, and decreasing disc thickness. In the absence of laser, the mean de-bonding values of discs cemented by a total etch adhesive system are always higher than those of discs cemented with a self-etch adhesive system. Without any extra load, all 0.5mm thick discs were dislodged from teeth while applying or testing the laser.en_US
dc.identifier.citationYılmaz, B. D., Polat, Z. S., İzgi, A. D., Gündüz, D. T., ve Dirihan, R.S. (2019). The contribution of ceramic thickness and adhesive type on the de-bonding strength of dental ceramic veneers using er,cr:Ysgg laser. Journal of Oral Research, 8(2), 131-139.en_US
dc.identifier.doi10.17126/joralres.2019.021en_US
dc.identifier.endpage139en_US
dc.identifier.issue2en_US
dc.identifier.scopus2-s2.0-85068747110en_US
dc.identifier.scopusqualityN/Aen_US
dc.identifier.startpage131en_US
dc.identifier.urihttp://www.joralres.com/index.php/JOR/article/view/joralres.2019.021/683
dc.identifier.urihttps://hdl.handle.net/11468/9774
dc.identifier.volume8en_US
dc.indekslendigikaynakScopusen_US
dc.institutionauthorYılmaz, Berivan Dündar
dc.institutionauthorPolat, Zelal Seyfioǧlu
dc.institutionauthorİzgi, Ayça Deniz
dc.language.isoenen_US
dc.publisherUniversidad de Concepcionen_US
dc.relation.ispartofJournal of Oral Researchen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectCeramicsen_US
dc.subjectDental debondingen_US
dc.subjectDental veneersen_US
dc.subjectErbium-doped yttrium aluminum garneten_US
dc.subjectLasersen_US
dc.subjectTooth preparationen_US
dc.titleThe contribution of ceramic thickness and adhesive type on the de-bonding strength of dental ceramic veneers using er,cr:Ysgg laseren_US
dc.title.alternativeLa contribución del espesor de la cerámica y el tipo de adhesivo a la resistencia de desunión de las carillas dentales de cerámica con láser Er, Cr: YSGGen_US
dc.typeArticleen_US

Dosyalar

Orijinal paket
Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
The contribution of ceramic thickness and adhesive type on the de-bonding strength of dental ceramic veneers using Er,Cr YSGG laser.pdf
Boyut:
334.17 KB
Biçim:
Adobe Portable Document Format
Açıklama:
Makale Dosyası
Lisans paketi
Listeleniyor 1 - 1 / 1
[ X ]
İsim:
license.txt
Boyut:
1.44 KB
Biçim:
Item-specific license agreed upon to submission
Açıklama: